Application/properties:
Austenitic-ferritic welding rod for TIG welding of high alloy steels to unalloyed steels. Highest operating temperature is 300˚C.
C | Si | Cr | Mn | Ni |
---|---|---|---|---|
<0.030 | 0.65-1 | 23-25 | 1-2.5 | 12-14 |
Shielding gas: 100% Ar
Tensile Strength ( N/mm 2 ) | 0.2% Proof Stress ( N/mm 2 ) | Elongation Lo = 4d% | Impact energy (J) ISO -V 25°C+ |
---|---|---|---|
>520 | >400 | >30 | >47 |
DIN Standard | 1.4406 X2CrNiMoN 17 12 2; 1.4401 X5CrNiMo 17 12 2; 1.4404 X2CrNiMo 17 13 2 G-X2CrNiMoN 18 10; 1.4311 X2CrNiN 18 10 |
Other Standard | ASTM/ACI A240/A312/A351: (TP)304LN; (TP)304L; CF-3; (TP)304 |
Delivery: welding rods
weight: 5 kg
diameter : 1 – 4 mm
Length: 1000 mm
Note : other weight & sizes are prodeced upon customers request