E 308–16
AWS/ASME SFA – 5.4 :E 19 9 R 26
DIN 8556 :E 19 9 R 12
prEN 1600 :Application/properties:
This electrode is suitable for welding of austenitic stainless Cr-Ni-Steels, as well as for temperatures up to +350°C; non-scaling up to +800°C. Some of its properties are fine-droplet metal transfer, good wash-in of joint sides, finely-rippled bead surface, easily removable slag, easy arc striking and restriking.
Weld metal analysis in % (typical values):
C | Mn | Si | Cr | Ni |
---|---|---|---|---|
0.04 | 0.8 | 0.9 | 19 | 10 |
Mechanical Properties of all-weld metal:
(Single values are typical values)
Tensile Strength (N/mm²) | Yield Strength 0.2% (N/mm²) | Elongation A5 (%) | Impact Energy (J) ISO-V +20°C |
---|---|---|---|
580 | 400 | 35 | 65 |
Welding Parameters | ||
---|---|---|
Diameter (mm) | Length (mm) | Amperage (A) |
2.5 | 250 | 45 – 80 |
3.25 | 300 – 350 | 70 – 120 |
4.0 | 350 | 100 – 150 |
5.0 | 350 | 130 – 230 |
Materials:
DIN EN Standard | 1.4306 X2CrNi 19 11 G-X2CrNiN 18 9; 1.4301 X5CrNi 18 10; 1.4311 X2CrNiN 18 10; 1.4312 G-X10CrNi 18 8; 1.4541 X6CrNiTi 18-10; 1.4546 X5CrNiNb 18-10; 1.4550 X6CrNiNb 18 10; 1.4303 X4CrNi 18 12; 1.4306 X2CrNi 19 11; 1.4308 G-X6CrNi 18 9; 1.4310 X12CrNi 17 7; 1.4319 X5CrNi 18 7 |
Other Standard | AISI 304, 304L, 304LN, 302, 321, 347; ASTM A157 Gr. C9; A320 Gr. B8C |
Rebaking: required at 350°C to 400°C for 2 hours.