Application/properties:
Rutile-Basic electrode is suitable for welding structural steels. Having a slow Si-content, Weld metal is particularly suited for subsequent galvanizing.
C | Si | Mn |
---|---|---|
0.08 | 0.2 | 0.6 |
(single values are typical values)
Tensile Strength ( N/mm 2 ) | Yield Strength ( N/mm 2 ) | Elongation A5 (%) | Impact energy (J) ISO -V 20°C -20°C+ |
---|---|---|---|
450– 550 | > 360 | > 22 | 100 70 |
Welding Parameters | ||
---|---|---|
Diameter (mm) | Length (mm) | Amperage (A) |
2.5 | 300 | 70 – 90 |
3.25 | 350 | 100 – 150 |
4 | 350 | 140 – 190 |
5 | 450 | 220 – 260 |
DIN Standard | St 37-2 to St 44-2; St 37-0 to St 52-0; St 37.4 to St 52.4; StE 210.7 to StE 360.7; StE 210.7 TM to StE 360.7 TM; St 35.8 to St 45.8; HI; HII; 17mn 4; WSTE 380;GS-38;GS52. |
EN Standard | S235JR to S275JR; P235T1 to P355T1; P235T2; P355T2; L210 to L360NB; L290MB to L360MB; P235G1TH; P255G1TH; P235GH; P265GH; P295GH, P255NH – P355NH |
ASTM Standard | ASTM A36 a.A53 Gr. all; A106 Gr. A, B, C, A 135 Gr. A, B, A283 Gr. A, B, C, D; A366; A285 Gr. A, B, C; A500 Gr. A, B, C; A570 Gr. 30, 33, 36, 40, 45; A607 Gr.45; A668 Gr. A, B, A907 Gr. 30, 33, 36, 40; A935 Gr.45; A936 Gr. 50. |
APl 5 L Gr. B, X42-X46 |
If necessary 1 hour at 100°C – 120°C