Application/properties:
Electrode for welding of stabilized austenitic stainless Cr-Ni-Mo steels or cast steels. Suitable for operating temperatures up to +400°C.Fine droplet metal transfer, good wash-in of joint sides, finely-rippled beat surface, easily removable slag. Easy arc striking and restriking.
C | Mn | Si | Cr | Ni | Mo | Nb |
---|---|---|---|---|---|---|
0.025 | 0.8 | 0.9 | 18.5 | 12 | 2.7 | 0.4 |
(single values are typical values)
Tensile Strength ( N/mm 2 ) | Yield Strength 0.2% ( N/mm 2 ) | Elongation A5 (%) | Impact energy(j) ISO - V 20°C+ |
---|---|---|---|
630 | 450 | 30 | 60 |
OCV>50V
Welding Parameters | ||
---|---|---|
Diameter (mm) | Length (mm) | Amperage (A) |
2.5 | 250 | 45 – 80 |
3.25 | 300 - 350 | 70 – 120 |
4.0 | 350 | 100 – 150 |
5.0 | 350 | 140 – 210 |
DIN EN standard | 1.4401 X5CrNiMo 17 122; 1.4406 X2CrNiMoN 17 122; 1.4408 G-X6CrNiMo 1810 ; 1.4436 X5CrNiMo 17 13 3; 1.4581 G-X5CrNiMoNb 18 10 ; 1.4571 X6CrNiMo Ti 17 12 2; 1.4580 X6CrNiMoNb 17 12 2; 1.4583 X 10CrNiMoNb 18 12 |
Other Standard | AISI 316L, 316Ti, 316Cb |
required at 350°C to 400°C for 2 hours.