E 309 MoL-16
AWS/ASME SFA – 5.4:1.4459
Comparable No. of materialE 23 13 2 L R 26
DIN 8556 :E 23 12 2 L R 12
EN 1600:Application/properties:
This electrode is used for joining of dissimilar steels, (austenitic steels to ferritic steels) and for depositing claddings austenitic. Weld metal consists of with approximately 15% delta-ferrite. Claddings on alloyed or low-alloyed steel are already corrosion resistant in the first layer. Highest operating temperature for dissimilar steel joints is +300°C at higher temperature AMA 1604G electrode shall be used. Fine droplet metal transfer, good wash-in of joint sides, finely-rippled bead surface, easily removable slag, easy arc striking and restriking are some properties of this electrode.
| C | Mn | Si | Cr | Ni | Mo |
|---|---|---|---|---|---|
| 0.025 | 0.9 | 0.7 | 22.5 | 13.5 | 2.6 |
(single values are typical values)
| Tensile Strength ( N/mm 2 ) | Yield Strength 0.2% ( N/mm 2 ) | Elongation A5 (%) | Impact energy(j) ISO - V 20°C+ |
|---|---|---|---|
| 640 | 420 | 30 | 50 |
| Welding Parameters | ||
|---|---|---|
| Diameter (mm) | Length (mm) | Amperage (A) |
| 2.5 | 250 | 60 – 90 |
| 3.25 | 300-350 | 90 – 120 |
| 4.0 | 350 | 100 – 160 |
| 5.0 | 350 | 140 – 210 |

OCV>70V

| DIN EN standard | 1.4401 X5CrNiMo 17 12 2; 1.4404 X2CrNiMo 17 13 2; 1.4429 X2CrNiMoN 17 13 3; 1.4406 X2CrNiMoN 17 12 2; 1.4408 G-X6CrNiMo 18 10; 1.4436 X5CrNiMo 17 13 3; 1.4581 G-X5CrNiMoNb 18 10; 1.4435 X2CrNiMo 18 14 3; 1.4436 X5CrNiMo 17 13 3; 1.4571 X6CrNiMoTi 17 12 2; 1.4573 X10CrNiMoTi 18 12; 1.4580 X6CrNiMoNb 17 12 2 G-X10CrNiMoNb 18 10 |
| Other Standard | ASTM/ACI A240/A312/A351: (TP)316L; CF-3M; (TP)316L; (TP)316LN; (TP)316; 316Ti; 316Ti; 316Cb |
required at 350°C to 400°C for 2 hours.