Application/properties:
Electrode for producing crack-free and tough welded joints in bellow temperature. Weld metal is extremely metallurgical purity having very low hydrogen content. Welds are of X-ray quality.
C | Mn | Si | Ni | S | P |
---|---|---|---|---|---|
0.05 | 0.7 | 0.4 | 3.2 | <0.02 | <0.02 |
(single values are typical values)
Tensile Strength ( N/mm 2 ) | Yield Strength ( N/mm 2 ) | Elongation A4 (%) | Impact energy (J) ISO - V 20°C -60°C -101°C+ |
---|---|---|---|
531 | 447 | 29 | >180 >100 >27 |
Welding Parameters | ||
---|---|---|
Diameter (mm) | Length (mm) | Amperage (A) |
2.5 | 350 | 65 – 95 |
3.25 | 350-450 | 90 – 140 |
4.0 | 350 | 140 – 185 |
5.0 | 450 | 180 – 250 |
DIN Standard | STE 285 to STE 420; 10Ni14; TSTE 225 to TSTE 380; 11 MnNi 5 3; 13 MnNi 6 3; 15 NiMn 6 |
EN Standard | 12Ni 14; S275 to S420; P275 – P420; S275Nto S420N; S275NL to S420NL; S355, S420; L360, L415, L445. |
ASTM Standard | A633 Gr. E; A572 Gr. 65; A203 Gr. D; A333 Gr. 3; A334 Gr. 3. |
required at 300°C to 350°C for 2 hours