Application/properties:
Electrodefor producing crack-free and tough welded joints. Weld metal is extremely metallurgical purity having very low hydrogen content. Welds are of X-ray quality.
C | Mn | Si | Ni | Mo |
---|---|---|---|---|
0.05 | 1.50 | 0.30 | 1.2 | 0.35 |
(single values are typical values)
Tensile Strength ( N/mm 2 ) | Yield Strength ( N/mm 2 ) | Elongation A5 (%) | Impact energy (J) ISO - V 20°C -60°C+ | Heat treatment |
---|---|---|---|---|
630 - 720 | >560 | >20 | 160 70 | AW |
620 - 720 | >550 | >20 | 150 55 | SR |
AW: As Welded
SR: Stress – Relieved 15 hours. /580°C
Welding Parameters | ||
---|---|---|
Diameter (mm) | Length (mm) | Amperage (A) |
2.5 | 350 | 65 – 95 |
3.25 | 450 | 90 – 140 |
4.0 | 450 | 140 – 185 |
5.0 | 450 | 180 – 240 |
DIN Standard | STE 420 to STE 500; WSTE 355 to WSTE 500; TSTE 420 to TSTE 500; 17MnMoV 6 4; 15NiCuMoNb 5; 20MnMoNi 4 5; . |
EN Standard | S420N to S500N; S355NL to S500NL; P355NL1 to P640NL1; P355NH to P500NH. |
ASTM Standard | ASTM A517 Gr. A, B, C, E, F, H, J, K, M, P. A225 Gr. C; A633 Gr. E; A572 Gr. 65 |
required at 300°C to 350°C for 2 hours