Application/properties:
Basic electrode with low carbon weld metal, suitable for resistant and hydrogen resistant steels (boilers, vessels and pipes), up to working temp of 600°C. Its weld metal is tough and resistant to work embitterment.
C | Mn | Si | P | S | Cr | Mo | V |
---|---|---|---|---|---|---|---|
0.05 - 0.12 | <0.9 | <0.4 | <0.02 | <0.02 | 1 - 1.5 | 0.4 - 0.65 | 0.1 - 0.35 |
(single values are typical values)
Tensile Strength ( N/mm 2 ) | Yield Strength ( N/mm 2 ) | Elongation A4,(%) | Impact energy (J) ISO - V 20°C+ |
---|---|---|---|
>540 | > 440 | >17 | >100 |
Welding Parameters | ||
---|---|---|
Diameter (mm) | Length (mm) | Amperage (A) |
2.5 | 350 | 60 – 85 |
3.25 | 450 | 100– 135 |
4.0 | 450 | 140 – 185 |
5.0 | 450 | 180 – 220 |
DIN Standard | 13CrMo 4 5, 25 CrMo 4, 14 CrMo 4 5, 16MnCr 5, ST37.3-ST52.3; STE 290.7-STE 415.7 |
EN Standard | S235J2G3; S355J2G3; L290NB- L415NB;L290MB ;P235GH |
ASTM Standard | A182 Gr. F12-1; A213 Gr.T12; A250 Gr.T12; A355 Gr.P12; A387 Gr. 11, 12; A506 Gr.4130; A507 Gr.4130; A513 Gr.4130; A519 Gr. 4130; A752 Gr.4130; A866 Gr.4130. |
required at 300°C to 350°C for 2 hours