Application/properties:
Basic electrode for producing crack-free and tough welded joints in low temperatures. Weld metal is of high metallurgical purity with very low hydrogen content. Easy releasable slag and good bead profile.
C | Mn | Si | Mo | Ni | S | P |
---|---|---|---|---|---|---|
0.07 | 1.7 | 0.45 | 0.35 | 0.5 | <0.02 | <0.02 |
(single values are typical values)
Tensile Strength ( N/mm 2 ) | Yield Strength ( N/mm 2 ) | Elongation A4 (%) | Impact energy (J) ISO - V 20°C -40°C -51°C+ | Heat treatment |
---|---|---|---|---|
630 - 780 | >550 | >22 | >130 >50 >40 | - |
630 - 760 | >550 | >22 | >130 >50 >40 | T |
T: Tempered 1 hour at 620°C, air cooling
Welding Parameters | ||
---|---|---|
Diameter (mm) | Length (mm) | Amperage (A) |
2.5 | 350 | 65 – 90 |
3.25 | 350 | 90 – 130 |
4.0 | 450 | 140 – 180 |
5.0 | 450 | 190 – 230 |
DIN Standard | STE 355 to STE 500; TStE 355 to TStE 500; 17MnMoV 6 4; 17MnNi 4; |
EN Standard | S380N; S500N; P380NL to S500NL. |
ASTM Standard | A517 Gr. A, B, C, E, F, H, J, K, M, P. A225 Gr. C; A633 Gr. E; A572 Gr. 65 |
Required at 300°C to 350°C for 2 hours
Preheating, inter pass temperature and post weld heat treatment in accordance with base metal to be welded.