Application/properties:
Basic electrode with low carbon weld metal , suitable for creep resistant and hydrogen resistant steels (boiler, vessels and pipes) up to working temperature of 600°C. Its weld metal is tough and resistant to work embitterment.
C | Mn | Si | P | S | Cr | Mo |
---|---|---|---|---|---|---|
<0.05 | 0.7 | 0.3 | <0.02 | <0.02 | 2.3 | 1 |
(single values are typical values)
Tensile Strength ( N/mm 2 ) | Yield Strength ( N/mm 2 ) | Elongation A5 (%) | Impact energy (J) ISO - V 20°C+ | Heat treatment |
---|---|---|---|---|
>550 | > 460 | > 17 | 120 | T |
T: Tempered 1 hour at 790°C, furnace cooling to 300°C
Welding Parameters | ||
---|---|---|
Diameter (mm) | Length (mm) | Amperage (A) |
2.5 | 350 | 60 – 90 |
3.25 | 450 | 100 – 140 |
4.0 | 450 | 140 – 180 |
5.0 | 450 | 190– 230 |
DIN Standard | 10CrMo9 10; 10CrSiMoV7; G17CrMo9; GS-12CrMo 9 10 |
ASTM Standard | A181 Gr. F22; A217 Gr.WC9; A335 Gr.P22; A336 Gr.F22. |
required at 300°C to 350°C for 2 hours