SMAW Electrodes

AMA 1263NR

  • E 8018–B2–H4R

    AWS/ASME SFA-5.5
  • E CrMo 1 B 20+

    DIN 8575:
  • E CrMo 1 B 42 H 5+

    prEN1599:
Download Catalog

Application/properties:

Basic electrode that uses nano technology in a humid environment with 80% humidity, the electrode coating is resistant to moisture absorption for 9 hours. This electrode is suitable for welding of creep resistant and high-pressure hydrogen resistant steels used in the construction of pressure vessels, boilers and piping subjected to operating temperatures up to +570°C. Welds are of X-ray quality.Preheating, interpass temperature and post-weld heat treatment in accordance with base metal to be welded.

Weld metal analysis in % (typical values):

CMnSiCrMo
0.060.800.401.000.50

Mechanical Properties of all-weld metal:

Tensile Strength
( N/mm )
Yield Strength
( N/mm )
Elongation
(5*d) (%)
Impact energy (J)
ISO - V
20°C+
Heat treatment
560 - 660> 490>22120T
450 - 550> 300>26150N+T

(single values are typical values)

T:  Tempered 0.5 hour at 700°C, air cooling

N+T:  Normalized + tempered 0.5 hour at 920°C, air cooling + 0.5 hour at 700°C

Welding Parameters
Diameter (mm)Length (mm)Amperage (A)
2.535060 - 85
3.25450100 - 130
4.0450140 - 180
5.0450190 - 230

 

Materials:

DIN Standard13CrMo 44; 15CrMo 5; 16CrMo 44; 25CrMo 4; 24CrMo 5; GS-22CrMo 54; GS-17CrMo 55  
EN Standard13CrMo 4-5; 15CrMo 5; 42CrMo 4; 16CrMoV 4; 25CrMo 4; 24CrMo 5; G22CrMo 5-4; G17CrMo 5-5  
ASTM StandardA193 Gr. B7; A335 Gr. P11 a. P12; A217 Gr. WC6  

Remarks:

  • Just Consume Dry Electrode
  • Rebaking: required on 300°C to 350°C for 2 hours.