Application/properties:
Electrode for welding of creep resistant and high-pressure hydrogen resistant steels used in the construction of pressure vessels, boilers and piping subjected to operating temperatures up to+550°C. Welds are of X-ray quality.
Preheating, inter-pass temperature and post-weld heat treatment in accordance with base metal to be welded.
C | Mn | Si | Mo |
---|---|---|---|
0.06 | 0.80 | 0.50 | 0.50 |
(single values are typical values)
Tensile Strength ( N/mm 2 ) | Yield Strength ( N/mm 2 )(%) | Elongation A5,(%) | Impact energy (J) ISO - V 20°C+ | Heat treatment |
---|---|---|---|---|
520 - 650 | > 470 | >22 | 160 | T |
T: Tempered 1 hour at 620°C, air cooling
Welding Parameters | ||
---|---|---|
Diameter (mm) | Length (mm) | Amperage (A) |
2.5 | 350 | 65 – 90 |
3.25 | 450 | 90– 130 |
4.0 | 450 | 140 – 180 |
5.0 | 450 | 190 – 230 |
DIN Standard | St 37-3 to St 52-3; St 37-2 to St 60-2; St 35.8 to St 45.8; StE 320.7 to StE 415.7; StE 255 to StE 500; 17 Mn 4; 19 Mn 5; 15 Mo 3; TStE 255 to TStE 500. |
EN Standard | S355J2G3; E295; E355; P255G1TH; L320 to L415NB; L320MB to L415MBM; S255N to S500N; P295GH; P310GH; 16Mo3; 15NiCuMoNb5, 20MnMoNi4-5; 17MnMoV6-4; S255NH to S500NH; S255NL to S500NL. |
ASTM Standard | A204 Gr.A, B, C; A217 Gr.WC1; A213 Gr.T2; A355 Gr.P1; A182M Gr.F1; A204M Gr.A, B, C; A250 Gr.T1 APl Spec. 5 L : X52, X56, X60 |
required at 300°C to 350°C for 2 hours.