Coated electrodes for manual welding

AMA 1230FR

  • E 7018–H4R

    AWS/ASME SFA – 5.1 :
  • E 51 54 B 5

    DIN 1913 :
  • E 42 4 B 42 H 5

    EN 499 :
  • E 425 B 42 H 5

    ISO 2560 :
Download Catalog

Application/properties:

Basic electrode that uses nano technology in a humid environment with 80% humidity, the electrode coating is resistant to moisture absorption for 9 hours. This electrode is suitable for producing crack-free and tough welding joints; weld metal recovery is approx 115%.

Weld metal analysis in % (typical values):

C Mn Si S P
0.07 1.4 0.55 < 0.02 < 0.02

Mechanical Properties of all-weld metal:

(single values are typical values)

Tensile Strength (N/mm²)Yield Strength (N/mm²)Elongation A5 (%)Impact Energy (J) ISO-V
+20°C-30°C
500 - 640> 420> 22> 16090
Welding Parameters
Diameter (mm) Length (mm) Amperage (A)
2.5 350 65 - 90
3.25 450 100 - 140
4.0 450 140 - 190
5.0 450 190 - 250
6.0 450 260 - 340

Materials:

DIN StandardSt 37-2 to St 60-2; St 37-3 to St 52-3; St 37.0 to St 52.0; St 37.4 to St 52.4; StE 210.7 to StE 360.7; StE 210.7 TM to StE 360.7 TM; St 35.8 to St 45.8; HI; HII; 17Mn4; GL-A 36 to GL-E 36; StE 255 to StE 355; WStE 255 to WStE 355; TStE 255 to TStE 355; TT ST 35 N; GS-38; GS-52
EN StandardS235JR to E335; S235J2G3 to S355J2G3; P235T1 to P355T1; P235T2; P355T2; L210 to L360NB; L290MB to L360MB; P235G1TH; P255G1TH; P235GH; P265GH; P295GH; S355G1S to S355G3S; S255N to S355N; P255NH to P355NH; S255NL to S355NL
ASTM StandardA27 a. A36 Gr. all; A214; A 242 Gr. 1-5; A 266 Gr. 1, 2, 4; A283 Gr. A, B, C, D; A285 Gr. A, B, C; A 299 Gr. A, B; A328; A366; A515 Gr. 60, 65, 70; A516 Gr. 55; A570 Gr. 30, 33, 36, 40, 45; A 572 Gr. 42, 50; A606 Gr. all; A607 Gr. 45; A656 Gr. 50, 60; A668 Gr. A, B; A907 Gr. 30, 33, 36, 40; A841; A851 Gr. 1, 2; A935 Gr. 45; A936
API 5 L Gr. B, X42 – X56;Gr. 50

Remarks:

  • Just Consume Dry Electrode
  • Rebaking: required on 300°C to 350°C for 2 hours.