SMAW Electrodes

AMA 1282NR

  • E 8018–G–H4R

    AWS/ASME SFA – 5.5 :
  • E Y 5076 Mn 1 Ni B H5

    DIN 8529 :
  • E 50 6 Mn 1 Ni B 42 H5

    EN 499 :
Download Catalog

Application/properties:

basic electrode with nanomaterials is resistant to moisture absorption for 9 hours in humid environments with 80% humidity.

This electrode used for welding fine-grained steels used in pressure vessels, boilers, pipes, steel structures, dam construction and shipbuilding. Its weld is tough and crack-resistant and has low hydrogen content. The electrode has a stable and concentrated arc, thus being well-suited or positional welding. Welds are of X-ray quality.

Weld metal analysis in % (typical values):

CMnSiNi
0.061.60.500.5

Mechanical Properties of all-weld metal:

Tensile Strength
( N/mm )
Yield Strength
( N/mm )
Elongation
A5 (%)
Impact energy (J)
ISO - V
20°C       -60°C+
590 - 690>510>23200          60

(single values are typical values)

Welding Parameters
Diameter (mm)Length (mm)Amperage (A)
2.535065 - 95
3.2545090 - 135
4.0450140 - 180
5.0450190 - 240

 

Materials:

DIN StandardStE420 to StE500; St 37-3 to St 52-3; WStE 420 to WStE 500; TStE 255 to TStE 500; StE240.7 TM to StE 445.7 TM; StE210.7 to StE445.7; EStE255 to EStE460  
EN StandardS255N to S355N; S235J2G3 to S355J2G3; P255NH to P500NH; S255NL to S500NL; L245MB to L450 MB; L210 – L450NB; E295 to E335; P355NL 1 to P460NL 1; S380N to S460N; P355NH to P460NH; S380NL to S460NL; S255NL 1 to S420NL 1  
ASTM StandardA516 Gr. 65; A572 Gr. 55, 60, 65; A633 Gr. E; A612; A618 Gr. I; A537 Gr. 1-3; A678 Gr. A-D  

Remarks:

  • Just Consume Dry Electrode
  • Rebaking: required on 300°C to 350°C for 2 hours.

Contact