E 309 L–15
AWS/ASME SFA – 5.4:E 2312 L B 20+
DIN 8556 :E 2312 L B 42
EN 1600:1.4332
Comparable No. of materialApplication/properties:
Basic electrode for joining of dissimilar steels, (austenitic steels to ferritic steels) and for depositing claddings austenitic. Weld metal consists of with approximately 15% delta-ferrite. Claddings on alloyed or low-alloyed steel are already corrosion resistant in the first layer. Highest operating temperature for dissimilar steel joints is +300°C; at higher temperature AMA 1604G electrode shall be used. The electrode has a stable arc.
| C | Mn | Si | Cr | Ni |
|---|---|---|---|---|
| 0.025 | 1 | 0.5 | 24 | 13 |
(single values are typical values)
| Tensile Strength ( N/mm 2 ) | Yield Strength 0.2% ( N/mm 2 ) | Elongation A5 (%) | Impact energy(j) ISO - V 20°C+ |
|---|---|---|---|
| 600 | 400 | 34 | 75 |

| Welding Parameters | ||
|---|---|---|
| Diameter (mm) | Length (mm) | Amperage (A) |
| 2.5 | 250 | 60 – 90 |
| 3.25 | 350 | 90 – 120 |
| 4.0 | 350 | 100 – 160 |
| 5.0 | 350 | 140 – 210 |

| DIN EN standard | 1.4406 X2CrNiMoN 17 12 2; 1.4401 X5CrNiMo 17 12 2; 1.4404 X2CrNiMo 17 13 2 G-X2CrNiMoN 18 10; 1.4311 X2CrNiN 18 10 |
| Other Standard | ASTM/ACI A240/A312/A351: (TP)304LN; (TP)304L; CF-3; (TP)304 |
required at 300°C for 2 hours.