Application/properties: electrode for producing crack-free and tough welding joints, also suited for welding steels having a carbon content of up to 0.6%. The weld metal has very low hydrogen content and is resistant to ageing. Approved for rail joint welding; Good gap bridging properties. the electrode has a stable and concentrated arc is therefore well suited for positional welding. Welds are if X-ray quality. CTOD-tested for offshore application.
Weld metal analysis in % (typical values):
P
S
Si
Mn
C
<0.02
<0.02
0.30
1.50
0.06
Mechanical Properties of all-weld metal: (Single values are typical values)
Heat Treatment
Impact Value (J)
ISO – V
Elongation
A5 (%)
Yield Strength
(N/mm2)
Tensile Strength
(N/mm2)
-60 ° C
+ 20 ° C
AW
70
180
> 22
> 420
500 – 640
SR
60
160
> 22
> 420
500 – 640
· AW: As-Welding
· SR: Stress-Reviled 15h/580°C
Welding Parameters
Amperage (A)
Length (mm)
Diameter (mm)
65 – 95
350
2.5
90 – 140
450
3.25
140 – 185
450
4.0
180 – 240
450
5.0
250 – 330
450
6.0
Materials:
St 37-2 to St 60-2; St 37-2 to St 52-3; St 37.0 to ST 52.0; St 37.4 to ST 52,4; StE 210.7 to StE 360,7; StE 210.7 TM toStE 360.7 TM; St 35.8 to St 45.8; HI; HII; 17mn 4; GL-A 36 to GL-E 36; StE 255 to StE 355; WStE 255 to WStE 355; TStE 255 to TStE 355; TT ST 35 N; GS-38; GS-52
DIN Standard
S235JR to E335; S235J2G3 to S355J2G3; P235T1 to P355T1; P235T2; P355T2; L210 to L360NB; L290MB to L360MB; P235G1TH; P255G1TH; P235GH; P265GH; P295GH; S355G1S to S355G3S; S255N – S355N; P255NH to P355NH; S255NL to S355NL.